Hi, what do you use as sand blocks for fairing?
I watched some tutorials but they were all about wood working. Wonder if there is some adjustment specific for composites.
So...
Wood (btw, with or without pads)?
Foam? Xps would be ok
Commercial available? Ifound permagrit blocks fantastic but they only make the coarser grits.

Thanks
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
There are plenty of sanding blocks on the market.  You can even make your own carved from a stiff foam (or even wood).  Sometimes if you have a fixed shape a custom block can be useful.  

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Warren (Staff) - 5/18/2020 4:28:46 PM
There are plenty of sanding blocks on the market.  You can even make your own carved from a stiff foam (or even wood).  Sometimes if you have a fixed shape a custom block can be useful.  

Thank you!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
             Thanks a lot!!
mporta71 - 5 Years Ago
Warren (Staff) - 5 Years Ago
             Thank you!
mporta71 - 5 Years Ago
scottracing - 5 Years Ago
mporta71 - 5 Years Ago
SleepingAwake - 5 Years Ago
mporta71 - 5 Years Ago
SleepingAwake - 5 Years Ago
                     Thank you, I will have a look at them!
mporta71 - 5 Years Ago
explorecomposites - 5 Years Ago
             Lot of ideas, thank you!
mporta71 - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search