Lester Populaire - 5/20/2020 11:53:24 AM
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.

Thank you Lester!
I don't own a 3D printer but considering to buy one.
Any recommendation?

Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Massimiliano - 5/20/2020 11:56:00 AM
Lester Populaire - 5/20/2020 11:53:24 AM
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.

Thank you Lester!
I don't own a 3D printer but considering to buy one.
Any recommendation?

I use Prusa printers privately and at work and only had good experiences with them. There are a lot cheaper printers that work well too but they are more of a toy than a tool i feel like. The Prusas are like the the cheapest option for a reliable workhorse.

Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Lester Populaire - 5/20/2020 12:17:05 PM
Massimiliano - 5/20/2020 11:56:00 AM
Lester Populaire - 5/20/2020 11:53:24 AM
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.

Thank you Lester!
I don't own a 3D printer but considering to buy one.
Any recommendation?

I use Prusa printers privately and at work and only had good experiences with them. There are a lot cheaper printers that work well too but they are more of a toy than a tool i feel like. The Prusas are like the the cheapest option for a reliable workhorse.

Thank you, I will have a look at them!

Chris Rogers
C
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 120, Visits: 933
You can cast-in-place sanding blocks with some packing tape on your surface, some polyester filler (Bondo) to take the surface shape and a wood backer to hold on to...

I'm a big fan of the 3M yellow foam blocks and the Stickit paper too - the blocks are hard enough yet have some give.  Not cheap but a great system.

You can also glue acrylic sheet to softer foam to make a flexible-yet-hard block for curved surfaces.  You want to sand (fair) with something that takes the shape of the surface you want to achieve - but no more - so you hit the high spots but don't over-sand the low ones.




Edited 5 Years Ago by Chris Rogers
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Chris Rogers - 5/22/2020 6:02:13 PM
You can also cast-in-place sanding blocks with some packing tape on your surface, some polyester filler (Bondo) to take the surface shape and a wood backer to hold on to...

I'm a big fan of the 3M yellow foam blocks and the Stickit paper too - the blocks are hard enough yet have some give.  Not cheap but a great system.

You can also glue acrylic sheet to softer foam to make a flexible-yet-hard block for curved surfaces.  You want to sand (fair) with something that takes the shape of the surface you want to achieve - but no more - so you hit the high spots but don't over-sand the low ones.

Lot of ideas, thank you!