ET 30 FAST HARDENER PROBLEM ????


Author
Message
Daz
Daz
Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)
Group: Forum Members
Posts: 93, Visits: 651
I have just got this off my shelf in the workshop to use,

I recently bought some new ,

now putting the bottles together the older one on the right looks a totally different colour to the new one,

Both of the bottles are unopened,

I keep them up on a shelf in the dark ,

What i want to know Is it still ok to use or not ??

Dont want to waste a lot of carbon and kevlar,

Any views on this ,

Thanks in advance.


Edited 14 Years Ago by Daz
Replies
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Daz,

You'll be fine. From the time the hardeners are manufactured, the material starts changing colour. It's not a function of UV exposure (which is why your hardeners have noth been stored in the dark but are now different colours), instead it will be the case that these two have been poured from two different barrels and would have been manufactured at slightly different times.

I'm totally confident that if we've supplied these in the last 12 months they will be perfectly fine to use and will both cure properly and fully.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Daz
Daz
Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)Supreme Being (906 reputation)
Group: Forum Members
Posts: 93, Visits: 651
Cheers Matt,

Have used it on a battery box lid and it has cured,