Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Tooling board would work, but it wouldn't be lightweight at all, especially the EB700 tooling board as it is a 700kg/M3 density - extremely heavy for use in a final component. You ideally want something no heavier than a 90-100kg/M3 density, but can also take high temperatures without inhibition... There aren't many options that spring to mind for me, but I would suggest it will be an aerospace product.
As Scott suggested, pre-preg may not be the most suitable choice for this one?
|