Hi I have  a new mould with 5 small parts in, they all have small but tightish curves in I worry that if I just lay carbon over it then vacuum it won't sit tidy into the mould.
Can I use spray glue the then lay the carbon into the curves, that's if I was the clear gel coat before the lay up.

My other question is do I need to clear gel coat? The mould is made from polyester gel coat. And worry it might stick using epoxy resin. I would easy lease and wax as if I was a new mould.

Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search