Group: Forum Members
Posts: 338,
Visits: 2K
|
Yes, a spray tack would be very useful. Cytec's Aerofix 3 works really well with EC's resins and leaves little or no trace if used sparingly, even on a 'bare' mould surface. Cutting your fabric into appropriately-sized pieces to can help get neat cosmetics if there's a likelihood that using a single piece of fabric will just pull and distort the weave, especially when dealing with significant changes in angle
Using an in-mould coating will also help ensure that your spray-tack is less likely to leave a residue and also give you a surface that's polishable, should there be any traces that you need to eliminate
|