MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K

Yes, a spray tack would be very useful. Cytec's Aerofix 3 works really well with EC's resins and leaves little or no trace if used sparingly, even on a 'bare' mould surface. Cutting your fabric into appropriately-sized pieces to can help get neat cosmetics if there's a likelihood that using a single piece of fabric will just pull and distort the weave, especially when dealing with significant changes in angle

Using an in-mould coating will also help ensure that your spray-tack is less likely to leave a residue and also give you a surface that's polishable, should there be any traces that you need to eliminate





carbon man
carbon man
Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Hi I have  a new mould with 5 small parts in, they all have small but tightish curves in I worry that if I just lay carbon over it then vacuum it won't sit tidy into the mould.
Can I use spray glue the then lay the carbon into the curves, that's if I was the clear gel coat before the lay up.

My other question is do I need to clear gel coat? The mould is made from polyester gel coat. And worry it might stick using epoxy resin. I would easy lease and wax as if I was a new mould.

Thanks