Message
f1rob
f1rob
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 237,
Visits: 4.8K
Might have some here mate what exact thickness are you looking for an what size ???
Reply
Like
2
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
was that with pre preg? I was looking for someone to make me some 2 ply sheet or just an offcut to make a new visor mount for my momo helmet, as I left all my glass sheets in germany and theres nothing thin enough at work
Reply
Like
3
morepower
morepower
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
It would be mostly down to the cure cycle you are using. Here I had to make a couple of single layer sheets.
This was just two sheets of glass with release film wrapped round it and then breather. The release was to just stop the excess resin being pulled into the breather.
Reply
Like
2
ChrisR
ChrisR
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
There's your problem, always apply to a cloth first then wipe onto the mould
Reply
Like
3
peter_lisica
peter_lisica
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 67
Thanks for the tips
Yes i do use gloves, but i don't change the cloth for each coat. And i'm pretty sure i applied a too heavy coat as i just sprinkle it on the glass and then wipe down.
Reply
Like
4
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
I found that is more of an application error. There's 3 main things that cause it:
1: Don't apply too heavy a coat. If you apply too much, the liquid will separate and leave streaks.
2: Do you wear gloves when you apply it? If not, the solvent in the Frekote dissolves the oils on your hands and deposits them on your tool surface leaving smears.
3: Similar problem if you don't use a new cloth to apply each coat, are you using the same cloth or getting a new one for every coat you apply? If you use the same cloth, you end up with the Frekote polymers drying on the cloth and then you apply more and the solvent partially dissolves the polymers again leaving a greasy residue on your tool surface.
The solution is to wear gloves, and use a new cloth for each coat. I like to cut my application wipes into 5 pieces so I don't go through a heap of them. Also make sure you clean the surface really well with solvent (preferably NOT acetone) to ensure any grease or residues that are already there don't get smeared around by the Frekote. Do these things and the Frekote will barely leave any residue at all, certainly not anything that transfers.
Reply
Like
4
peter_lisica
peter_lisica
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 67
Hy
now that i have a pin hole free surface i have another question.
Although the surface is smooth there are still some stripes visible from the release agent i think. I am using a frekote 770-nc.
Is there a way to get ride of this stripes on carbon fibre. And how/can I get rid of this problem when applying the release agent. I have tried polishing it with a smooth cloth by hand after the release agent has dried, but it seems that is not enough.
Thanks
Reply
Like
4
peter_lisica
peter_lisica
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 67
Thanks Rob,
I taped the edges, and straight to 120C at 3 bar and the result is outstanding
no pinholes, really perfect glossy finish on both sides.
Attachments
IMG_1851.JPG
(
1.5K views,
407.00 KB
)
IMG_1852.JPG
(
1.2K views,
371.00 KB
)
Reply
Like
4
f1rob
f1rob
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 237,
Visits: 4.8K
Well looking at the data sheet its a 42% resin material an a fairly standard cure (120,2 dag a minute ramp)
For a single ply you wouldn't need a dwell so straight to 120
but on glass you should be ok with 30psi to get the Finnish but still tape the edges off
Reply
Like
4
peter_lisica
peter_lisica
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 67
Hy the carbon fiber si twill 200g/m2, and the technical data sheet of the epoxy is here
http://www.delta-tech.it/pdf/STE%20DT120-6.pdf
What i found is that nearer the edges there are less and less pinholes, to about 2cm from the edge there are no pinholes left.
The main focus is that we get rid of this pinholes on both sides and is not important structuraly.
And another thing that i found out is when i put the glass panel on just one side, the surface was perfect and pinhole free.
How would you recomend the autoclau cycle (pressure and temperatures) to give the best chance of getting what i want.
And also i am wondering what is causing the pinholes. Is it gas forming in the epoxy that can't escape, or is it epoxy bleeding out.
F1rob
Yes the carbon fiber sheet is the same size as the glass panels but i didn't flash tape around so I Will try that also, if the problem is resin bleed.
Regards
Attachments
20150614_164517.jpg
(
978 views,
3.00 MB
)
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
1
2
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search