Hy




I have a problem, which i do not know how to solve. For my application i need a thin sheet of carbon fiber that is perfect finish on both sides.




I am using one layer of deltapreg 200g prepreg and vacuumed between two glass panells and than baked in autoclau on 4bar. The problem is no matter what i try i get pinholes on both sides, which are not acceptable. I have also tried with drg carbon with resin and the result is similar.




What can i do to get rid of the pinholes on both sides and get a perfect finish?



Reply
peter_lisica
peter_lisica
Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)
Group: Forum Members
Posts: 5, Visits: 67
Hy




now that i have a pin hole free surface i have another question.




Although the surface is smooth there are still some stripes visible from the release agent i think. I am using a frekote 770-nc.

Is there a way to get ride of this stripes on carbon fibre. And how/can I get rid of this problem when applying the release agent. I have tried polishing it with a smooth cloth by hand after the release agent has dried, but it seems that is not enough.




Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
peter_lisica - 10 Years Ago
Warren (Staff) - 10 Years Ago
peter_lisica - 10 Years Ago
f1rob - 10 Years Ago
f1rob - 10 Years Ago
peter_lisica - 10 Years Ago
peter_lisica - 10 Years Ago
Hanaldo - 10 Years Ago
peter_lisica - 10 Years Ago
ChrisR - 10 Years Ago
morepower - 10 Years Ago
scottracing - 10 Years Ago
f1rob - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search