By peter_lisica - 6/12/2015 12:34:13 PM

Hy




I have a problem, which i do not know how to solve. For my application i need a thin sheet of carbon fiber that is perfect finish on both sides.




I am using one layer of deltapreg 200g prepreg and vacuumed between two glass panells and than baked in autoclau on 4bar. The problem is no matter what i try i get pinholes on both sides, which are not acceptable. I have also tried with drg carbon with resin and the result is similar.




What can i do to get rid of the pinholes on both sides and get a perfect finish?


By f1rob - 11/24/2015 3:10:42 PM

Might have some here mate what exact thickness are you looking for an what size ???