It would be mostly down to the cure cycle you are using. Here I had to make a couple of single layer sheets. 



This was just two sheets of glass with release film wrapped round it and then breather. The release was to just stop the excess resin being pulled into the breather. 
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
was that with pre preg? I was looking for someone to make me some 2 ply sheet or just an offcut to make a new visor mount for my momo helmet, as I left all my glass sheets in germany and theres nothing thin enough at work Sad
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Might have some here mate what exact thickness are you looking for an what size ???