Small multiple part run in casting box using resin infusion process


Small multiple part run in casting box using resin infusion process
Author
Message
twissta
twissta
Supreme Being (319 reputation)Supreme Being (319 reputation)Supreme Being (319 reputation)Supreme Being (319 reputation)Supreme Being (319 reputation)Supreme Being (319 reputation)Supreme Being (319 reputation)Supreme Being (319 reputation)Supreme Being (319 reputation)
Group: Forum Members
Posts: 27, Visits: 341
Ok here is a question, I would like to know if it is possible to lay (4) small molds is a casting box, using the resin infusion process for a parts run, end result (4) parts ready for finishing.

Now take in consideration that everything is done properly, gel coating, bagging, correct amount of resin etc.

could you elaborate please.