Talk Composites - The Forum for Advanced Composites

Small multiple part run in casting box using resin infusion process

http://www.talkcomposites.com/Topic156.aspx

By twissta - 1/22/2012 5:38:28 AM

Ok here is a question, I would like to know if it is possible to lay (4) small molds is a casting box, using the resin infusion process for a parts run, end result (4) parts ready for finishing.

Now take in consideration that everything is done properly, gel coating, bagging, correct amount of resin etc.

could you elaborate please.
By Joe - 1/23/2012 10:46:36 PM

twissta (23/01/2012)

When the first one is finished I am going to post a pic, for all to see............Smile Whistling


Hell yeah, those first parts produced are a real pride... i think we would be interested too in having pics of the process u choose, if you dont mind.

Good luck Wink