Hello guys

can not understand or to find when i do work with vinilyster resin and i put piece into owen at what temperature and how many hours do i have to hold it?
as one guy told 2-3 hours at temperature 50-70 C , so i holded but took out parts surface hard but when to brush with paper like 100 its a little tacky like it was. do not get.