Hello guys

can not understand or to find when i do work with vinilyster resin and i put piece into owen at what temperature and how many hours do i have to hold it?
as one guy told 2-3 hours at temperature 50-70 C , so i holded but took out parts surface hard but when to brush with paper like 100 its a little tacky like it was. do not get.
Reply
Zorongo
Zorongo
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 40, Visits: 330
I´m not sarcastic, but you should read the technical data sheet. There´s a lot of chemistry involved on resins.... and each resin may be different from the other.. TDS will give you the especific needings for your resin. It´s your bible (with respect)

1 hour 25ºC should be enough if properly catalyzed (and accelerated ?). (again, TDS)

For the tacky surface MAY BE you´ll have to isulate surface from oxygen. But again, read TDS. Waxed styren may be added to resin to create a suface barrier isulating from the oxygen. Or a vac bag. Or cello plastic, or waxed gel coat (top coat)....

Good luck ! Wink
Edited 10 Years Ago by Zorongo
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search