Talk Composites - The Forum for Advanced Composites

vinylester resin curing

http://www.talkcomposites.com/Topic15397.aspx

By TomDesign - 3/6/2015 10:35:41 AM

Hello guys

can not understand or to find when i do work with vinilyster resin and i put piece into owen at what temperature and how many hours do i have to hold it?
as one guy told 2-3 hours at temperature 50-70 C , so i holded but took out parts surface hard but when to brush with paper like 100 its a little tacky like it was. do not get.
By TomDesign - 3/7/2015 6:16:09 AM

Thank you as bigger layers i layed like 2 large layers and at 50 c not enough was 2 hours. but when i put with one layer in 40c for 2 hours was already not bad. so keep trying.