Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
vinylester resin curing
vinylester resin curing
Post Reply
Like
2
vinylester resin curing
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Thank you as bigger layers i layed like 2 large layers and at 50 c not enough was 2 hours. but when i put with one layer in 40c for 2 hours was already not bad. so keep trying.
Reply
Like
2
Zorongo
Zorongo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 40,
Visits: 330
I´m not sarcastic, but you should read the technical data sheet. There´s a lot of chemistry involved on resins.... and each resin may be different from the other.. TDS will give you the especific needings for your resin. It´s your bible (with respect)
1 hour 25ºC should be enough if properly catalyzed (and accelerated ?). (again, TDS)
For the tacky surface MAY BE you´ll have to isulate surface from oxygen. But again, read TDS. Waxed styren may be added to resin to create a suface barrier isulating from the oxygen. Or a vac bag. Or cello plastic, or waxed gel coat (top coat)....
Good luck !
Edited
10 Years Ago by
Zorongo
Reply
Like
2
TomDesign
TomDesign
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Hello guys
can not understand or to find when i do work with vinilyster resin and i put piece into owen at what temperature and how many hours do i have to hold it?
as one guy told 2-3 hours at temperature 50-70 C , so i holded but took out parts surface hard but when to brush with paper like 100 its a little tacky like it was. do not get.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search