	Group: Forum Members 	        
    Posts: 93, 
    Visits: 651 
    
 
          
		     | 
				                       
                 
                
                    
			            I have a question for all the teck guys on here,
  I just infused a mold for one of the doors on my car, 
  Its now been 48 hrs since infusion and the resin is taking and age to go off,
  Now i know how important it is to mix the resin correctly as Matt explained to me its imperative to get the ratio 
  perfect and to mix it thoroughly.
  The only thing is my workshop is at 10 deg and has been for the last few days as i havnt been there ,
  Any idea how long its going to take at this temp for it to go off ????                
			            				
			                                 
                     
                                            
                         
                    
                  
             |