By Daz - 5/2/2012 11:13:56 PM

I have a question for all the teck guys on here,

I just infused a mold for one of the doors on my car,

Its now been 48 hrs since infusion and the resin is taking and age to go off,

Now i know how important it is to mix the resin correctly as Matt explained to me its imperative to get the ratio

perfect and to mix it thoroughly.

The only thing is my workshop is at 10 deg and has been for the last few days as i havnt been there ,

Any idea how long its going to take at this temp for it to go off ????
By Joe - 5/4/2012 2:02:49 PM

Hi Daz,

Mistakes happen, but at least you know what was wrong.

Happy to see some new panels coming Wink