resin infusion cure times ?


Author
Message
Daz
Daz
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 93, Visits: 651
I have a question for all the teck guys on here,

I just infused a mold for one of the doors on my car,

Its now been 48 hrs since infusion and the resin is taking and age to go off,

Now i know how important it is to mix the resin correctly as Matt explained to me its imperative to get the ratio

perfect and to mix it thoroughly.

The only thing is my workshop is at 10 deg and has been for the last few days as i havnt been there ,

Any idea how long its going to take at this temp for it to go off ????
Reply
Daz
Daz
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 93, Visits: 651
cheers kevin,

 I have found what i did wrong CryingAngry

I have the big tin of resin 30kg

I decanted some for the door

and picked up what i thought was the hardener looks like i made the wrong choicePinch

i mixed resin with the correct amount of resin Crying



That will teach me not to rush anymore even if i have to go to workAngryAngry

some scrap carbon in the bin


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search