Hi,
I have finally finished my first project. I thought I would start with something easy.
Brian.
Edited
12 Years Ago by
Brian_s
Reply
Like
7
Replies
FLD
FLD
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
Wow, that is stunning! Have you considered getting it pinstriped?
Reply
Like
7
Brian_s
Brian_s
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 99,
Visits: 2.5K
The tone is similar if not smoother and rounder. It also seems slightly louder.
It is hard to compare to my un-trained ear anyway.
I will do some recordings soon of the 2 harps. The strings are still stretching so it is going off tune quite quickly.
I have not thought about pin stripes. I have not thought of much except will it be strong enough and sound good.
There is about 700 lbs pull across all of the strings. I love the shape that the sound board has bowed into.
I am not sure if it is really and advantage but I used Twaron for the sound board. It seemed like a good idea to me.
Confirmation of a question I asked a long time ago. Yes. PT326 is strong enough to hold it.
Brian.
Reply
Like
7
Brian_s
Brian_s
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 99,
Visits: 2.5K
Sound files. I hope this works. I have never used soundcloud before.
Brian.
https://soundcloud.com/brian_sav/wooden-harp-wav
https://soundcloud.com/brian_sav/carbon-harp-wav
Reply
Like
7
ChrisR
ChrisR
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
the wooden one sounds more mellow, the CF one sounds a little "bright" but that may mellow once everything has settled.
Cool project though and ace result.... any more in the pipeline?
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Harp
Brian_s
-
12 Years Ago
Hi! This part is AMAZING, looks awesome. I think this is a good example when hard work paid off. Can...
wojtepanik
-
12 Years Ago
Yes it is made to be played. It sounds great. My wife has a wooden one that this is based on. As the...
Brian_s
-
12 Years Ago
Stunning :) Is the tone any different compared to the original? Warren
wozza
-
12 Years Ago
Hey, Been a while I did not post, but now I feel like it's time to. This piece is awesome in...
Joe
-
12 Years Ago
Wow, that is stunning! Have you considered getting it pinstriped?
FLD
-
12 Years Ago
The tone is similar if not smoother and rounder. It also seems slightly louder. It is hard to...
Brian_s
-
12 Years Ago
Sound files. I hope this works. I have never used soundcloud before. Brian....
Brian_s
-
12 Years Ago
the wooden one sounds more mellow, the CF one sounds a little "bright" but that may mellow once...
ChrisR
-
12 Years Ago
Hats off to an awesome project!!! congrats, sounds great too, although im no expert. cheers
baja_patient
-
12 Years Ago
Thank you all for your kind words. Chris, I think the problem with the sound is that the start of...
Brian_s
-
12 Years Ago
[quote][b]Brian_s (17/11/2013)[/b][hr]Hi, I have finally finished my first project. I thought I...
fgayford
-
12 Years Ago
To my ear, the Carbon Harp sounds brighter and has much more "sustain" on the strings than the...
Dravis
-
12 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search