By Brian_s - 11/17/2013 10:47:09 AM
Hi,
I have finally finished my first project. I thought I would start with something easy. 
Brian.




|
By Dravis - 11/27/2013 2:39:19 PM
To my ear, the Carbon Harp sounds brighter and has much more "sustain" on the strings than the wooden harp. Probably caused be a much stiffer frame.
(A friend and I built a couple of Carbon fibre reinforced electric Bass guitars back in the early 90'ies) we used the parts from a few damaged instruments,, (pickups, e.t.c.)
They had a much "drier" sound with more sustain than any wooden bass.. I think that sound "fell out of fashion" in the 00'es
|
|