Yes it is made to be played. It sounds great. My wife has a wooden one that this is based on. As the weather changes, the wood moves and it goes out of tune. I thought Carbon Fibre would be more stable. I am just waiting for the strings to settle down. (Nylon strings stretch and go out of tune for a few days.) Then I will record my wife playing it.

Cost, including making the moulds and vacuum equipment (I already had a vacuum pump.) are about £700 plus £70 for harp tuning pins and strings etc.

I have learned a lot from making this.

Brian.
Edited 12 Years Ago by Brian_s
wojtepanik
wojtepanik
Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)
Group: Forum Members
Posts: 102, Visits: 582
Hi!
This part is AMAZING, looks awesome. I think this is a good example when hard work paid off. Can you play it as normal Harp? If yes, please post some vid when you do! What was the cost of production? 
Bye!
Wojtek from Poland

~~~Everytime I hear sound of demoulding part I have eargasm~~~
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Hi,

I have finally finished my first project. I thought I would start with something easy.   Smile


Brian.









Edited 12 Years Ago by Brian_s
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search