To my ear, the Carbon Harp sounds brighter and has much more "sustain" on the strings than the wooden harp. Probably caused be a much stiffer frame.

(A friend and I built a couple of Carbon fibre reinforced electric Bass guitars back in the early 90'ies)  we used the parts from a few damaged instruments,, (pickups, e.t.c.)

They had a much "drier" sound with more sustain than any wooden bass.. I think that sound "fell out of fashion" in the 00'es  Wink

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
fgayford
fgayford
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Brian_s (17/11/2013)
Hi,

I have finally finished my first project. I thought I would start with something easy.   Smile


Brian.


Nice job Brian, it looks great and I think it sounds vastly superior to the wooden one!
The big bonus with making instruments in carbon fiber is that the voice is so much more powerful and loud.
Our violins and guitar both had this positive effect.
 Fred

Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Thank you all for your kind words.

Chris,
I think the problem with the sound is that the start of each note overwhelms the recorder. The real thing sounds better than the recording.
I am planning to make another harp similar to this one but with a rounded back sound box. It feels like cheating to make 4 sides a top and bottom and glue them together. OK in wood but you can do better with composites. Now I have more of a feel for the materials I am sure I can give it a better finish as well.
This weighs 3.6Kg. 3.2Kg lighter than the wooden one. Not knowing how strong is strong enough, I have pretty certainly put too much Carbon fibre in places.

Brian.
baja_patient
baja_patient
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Hats off to an awesome project!!! congrats, sounds great too, although im no expert.

cheers
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
the wooden one sounds more mellow, the CF one sounds a little "bright" but that may mellow once everything has settled.

Cool project though and ace result.... any more in the pipeline?
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Sound files. I hope this works. I have never used soundcloud before.

Brian.



https://soundcloud.com/brian_sav/wooden-harp-wav

https://soundcloud.com/brian_sav/carbon-harp-wav
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
The tone is similar if not smoother and rounder. It also seems slightly louder.
It is hard to compare to my un-trained ear anyway.
I will do some recordings soon of the 2 harps. The strings are still stretching so it is going off tune quite quickly.
I have not thought about pin stripes. I have not thought of much except will it be strong enough and sound good.
There is about 700 lbs pull across all of the strings. I love the shape that the sound board has bowed into.
I am not sure if it is really and advantage but I used Twaron for the sound board. It seemed like a good idea to me.
Confirmation of a question I asked a long time ago. Yes. PT326 is strong enough to hold it.

Brian. 
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Wow, that is stunning!  Have you considered getting it pinstriped?
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hey, 

Been a while I did not post, but now I feel like it's time to. 

This piece is awesome in every way. Oh well, gives me chills. 

Congrats, and as for the others, I'd be happy to hear how it sounds, compared to the wood one. 

 



 


    A $1000 electronic device will always protect a 10 cents fuse
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Stunning Smile Is the tone any different compared to the original?

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search