StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 380
I'd like to get the back part of my mould painted, but I've no idea how to get a smooth finish on that side of it (the peel ply side) Do I sand it down? Brush another layer of resin?
Reply
Like
4
Replies
StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 61,
Visits: 380
matthieutje65 (15/11/2013)
are you talking about the backpart of your mould or from the part?
If you mean the back of your mould, can I ask you why you would like to have it painted?
Because it's a cosmetic part (display tray) and needs a good finishing on both surfaces
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Makes it a bit more difficult...
You can sand the back where you had the peelply, add a new coat, sand and polish it...
Thats how I would do it or make a top and bottom mould.
Maybe some other members have other ideas?!
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Finishing the peel ply side of the mould
StanTheMan
-
12 Years Ago
are you talking about the backpart of your mould or from the part? If you mean the back of your...
matthieutje65
-
12 Years Ago
[quote][b]matthieutje65 (15/11/2013)[/b][hr]are you talking about the backpart of your mould or from...
StanTheMan
-
12 Years Ago
Makes it a bit more difficult... You can sand the back where you had the peelply, add a new coat,...
matthieutje65
-
12 Years Ago
Sand down and a couple of heavy coats of lacquer would be how I go for a one off
ajb100
-
12 Years Ago
There multiple ways: 1) sand and lacquer. This is how I'd do it for a one off 2) remould using a...
FLD
-
12 Years Ago
Hi! I think good way to do it is just to skin/wrap back layer with carbon - as they do in...
wojtepanik
-
12 Years Ago
if you want to smooth layer of backside, you can try add more release film between carbon fiber...
Vichaya
-
12 Years Ago
Sand and lacquer or sand and thin coat of resin are the two simplest methods.
Warren (Staff)
-
12 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search