By StanTheMan - 11/15/2013 9:10:54 AM
I'd like to get the back part of my mould painted, but I've no idea how to get a smooth finish on that side of it (the peel ply side) Do I sand it down? Brush another layer of resin?
|
By Warren (Staff) - 12/30/2013 11:45:10 AM
Sand and lacquer or sand and thin coat of resin are the two simplest methods.
|
|