Carbon fibre leg :)
Carbon fibre leg :)
Post Reply
Like
3
Carbon fibre leg :)
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
carbonfibreworks
carbonfibreworks
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Well not quite a full leg but one of my customers (and a good friend) had a problem with his plastic lower leg support so asked i could help him out. The result is an over engineered component with three layers of 450g carbon and one layer of Kevlar , it still weighs less than the part its replacing and is strong enough to be used on a baby elephant
All materials from EC . Please take note, making items like the one below must be done so with extreme caution and doing so without the correct knowledge/liability insurance etc could leave you open to litigation should it fail and cause injury. I am doing this as a request from a friend and will not be making the part on a commercial basis .
www.carbonfibreworks.co.uk
Edited
12 Years Ago by
carbonfibreworks
Reply
Like
3
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
Is this for drop foot?
I've got to do the same part for someone soon, we're just waiting for him to get his muscle back to cast the leg and then produce a bespoke support
Looks very good, does it flex much when walking?
Edited
12 Years Ago by
ajb100
Reply
Like
3
carbonfibreworks
carbonfibreworks
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Hi
Not sure of his medical condition, to say it is strong is an understatement i may have to produce another with a bit more flex
Chris
www.carbonfibreworks.co.uk
Edited
12 Years Ago by
carbonfibreworks
Reply
Like
3
LaxFriedrichs
LaxFriedrichs
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 58,
Visits: 450
Great stuff. How would you make the laminate more flexible?
Reply
Like
4
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Less layers = more flexible. Replace carbon with kevlar also would make it more flexible.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search