Well not quite a full leg but one of my customers (and a good friend) had a problem with his plastic lower leg support so asked i could help him out. The result is an over engineered component with three layers of 450g carbon and one layer of Kevlar , it still weighs less than the part its replacing and is strong enough to be used on a baby elephant Smile All materials from EC . Please take note, making items like the one below must be done so with extreme caution and doing so without the correct knowledge/liability insurance etc could leave you open to litigation should it fail and cause injury. I am doing this as a request from a friend and will not be making the part on a commercial basis .
www.carbonfibreworks.co.uk

 

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Edited 12 Years Ago by carbonfibreworks
Reply
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi
Not sure of his medical condition, to say it is strong is an understatement i may have to produce another with a bit more flex Smile
Chris
www.carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Edited 12 Years Ago by carbonfibreworks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search