What exactly is is the infusion mesh?


Author
Message
StanTheMan
StanTheMan
Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)
Group: Forum Members
Posts: 61, Visits: 380
I mean, is it just a regular nylon/plastic mesh that is found in places like B&Q or is it a specialized product made specifically for resin infusions?
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
It is something special to be able to have a good air/resin-flow and can not be replaced by any DIY-materials as far as I know...

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
From looking closely at the mesh, the vertical and horizontal strands of plastic are laid on top of each other meaning there is always a gap throughout the mesh.  I imagine the gap is key to resin flow.

A flat mesh with a tight fitting vacuum bag may well have minimal/no gaps and hence not flow well.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
wojtepanik
wojtepanik
Supreme Being (757 reputation)Supreme Being (757 reputation)Supreme Being (757 reputation)Supreme Being (757 reputation)Supreme Being (757 reputation)Supreme Being (757 reputation)Supreme Being (757 reputation)Supreme Being (757 reputation)Supreme Being (757 reputation)
Group: Forum Members
Posts: 102, Visits: 582
I saw in my shop some garden mesh that looked the same as inf mesh I think it would do the job pretty well Smile

~~~Everytime I hear sound of demoulding part I have eargasm~~~
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
The correct infusion mesh is not expensive when you break down the stack and all you consumables, the risk of ruining a component and the lost time stops me even considering using anything other that the correct materials. 
Chris
www.carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Daz
Daz
Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)
Group: Forum Members
Posts: 93, Visits: 651
its an inexpensive part of the stack so would just use the proper stuff you know that works perfect,