StanTheMan
StanTheMan
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 380
I mean, is it just a regular nylon/plastic mesh that is found in places like B&Q or is it a specialized product made specifically for resin infusions?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
What exactly is is the infusion mesh?
StanTheMan
-
13 Years Ago
It is something special to be able to have a good air/resin-flow and can not be replaced by any...
matthieutje65
-
13 Years Ago
From looking closely at the mesh, the vertical and horizontal strands of plastic are laid on top of...
Warren (Staff)
-
13 Years Ago
I saw in my shop some garden mesh that looked the same as inf mesh I think it would do the job...
wojtepanik
-
13 Years Ago
The correct infusion mesh is not expensive when you break down the stack and all you consumables,...
carbonfibreworks
-
13 Years Ago
its an inexpensive part of the stack so would just use the proper stuff you know that works perfect,...
Daz
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search