By StanTheMan - 10/5/2013 1:21:42 PM

I mean, is it just a regular nylon/plastic mesh that is found in places like B&Q or is it a specialized product made specifically for resin infusions?
By Daz - 10/13/2013 1:55:00 PM

its an inexpensive part of the stack so would just use the proper stuff you know that works perfect,