Another way for embossed logo's is to put a mirror image vinyl on the mould and release coat over it. You will likely need either a thicker vinyl or precisely place a few layers ontop of each other to get a deep recess.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|