Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Getting a logo on a finished CF part?
Getting a logo on a finished CF part?
Post Reply
Like
2
Getting a logo on a finished CF part?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
KeyboardWarrior
KeyboardWarrior
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 14
Hi,
Any suggestions as to how to put a great looking logo onto a finished carbon fibre part? I'm thinking a logo in silver should look good against the carbon fibre background.
I'm guessing silver wording on a clear adhesive label would do if quality wasn't an issue, but how would you go about it if the only concern was making the finished part look really professional?
Thanks in advance!
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Getting a logo on a finished CF part?
KeyboardWarrior
-
12 Years Ago
Hi, I use graphics quite a lot on my parts. I do it two ways. I invested in a Vinyl Plotter Cutter...
wozza
-
12 Years Ago
look at my posts i always put logos and stickers under resin. only do not ever put logo under...
TomDesign
-
12 Years Ago
Very helpful suggestions. Thank you.
KeyboardWarrior
-
12 Years Ago
Warren I'm glad you said that! I have been toying with the idea for a while as I use gc50 most of...
Ortonporton
-
12 Years Ago
Hi, I did a sign for outside the workshop 1m x 1m with 80mm high letters and that turned out ok. I...
wozza
-
12 Years Ago
Another way for embossed logo's is to put a mirror image vinyl on the mould and release coat over...
Warren (Staff)
-
12 Years Ago
Another method I use which is a bit more subtle is to use the vinyl graphics/ letters etc as a mask....
wozza
-
12 Years Ago
Just a note from a failure that may help someone else. I used a thermal transfer color print on...
Farbin Kaiber
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search