WOW!!!!! some amazing work i cant wait to get started playing around with some parts
FLD
FLD
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Here's my latest.  Its an instrument binnacle for a VX220.  I shouldv'e cleaned off the bits of polish I missed before I took the pics!




Edited 13 Years Ago by FLD
FLD
FLD
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Bit of a bodge but I moulded this on a piece of chipboard which I covered in vinyl.  Its an undertray for my car.  Its in 2 layers of spread tow (45 degrees), 3mm 3D core, 2 layers.  It weighs in at 3kg and is VERY rigid.


wozza
wozza
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi, I have been experimenting with colouring the GC50.
Attached are pics of the result.
The Red Edges where sprayed into the mould first followed by clear and then my normal infusion lay up.

Just added another pic of a Bonnet Scoop made using the same method

Regards Warren

Carbon Copies Ltd
Edited 13 Years Ago by wozza
FLD
FLD
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Looks good wozza.  How do you find spraying the coloured gel, does it have enough opacity or do you have to lay it on thick?
wozza
wozza
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Cheers, I added the pigment at a ratio of 10% and laid down my normal 0.2mm ish coat. 

The Red is fine with good colour depth. The white could do with a tad more pigment, if you look really really close you can just see a hint of the black carbon bleading through. 

It has taken quite a bit of time to get things rightWink Timing is crucial, pull the masking tape off too soon and you are left with a "rough" edge leave it too long and you lift the GC50 from the mouldCrying

Carbon Copies Ltd
Edited 13 Years Ago by wozza
FLD
FLD
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I consider 0.2mm damn thin!  I'm still brushing gelcoat and wetlaying.  I really should take the plunge into spraying and infusing Rolleyes
wozza
wozza
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
The problem with spraying on the GC50 is that if you lay it down too thick then you loose some of the clarity, the weave can start to look a bit blurred. Not as much of an issue on plain weave but quite noticeable on 2/2 twill.

Carbon Copies Ltd
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
I've been gradually making parts for my car in composites... finally got some lacquer on them so thought id post a few pics

The doors, front and rear end and headlights are made using resin infusion from moulds I made.... the roof is actually wrapped in pro finish carbon using easycomposites wrapping process.... in fact ALL the materials and advice for both the parts and moulds was from easycomposites who I cant recommend enough Smile






















Edited 13 Years Ago by andygtt
fgayford
fgayford
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Wozzo
Nice work, these parts look fantastic. I spray 2k clear the night before I infuse also.
Haven't tried color yet.
Fred
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search