unfortunately I cannot see the defects you were talking about with the print through... the last few photos look like an amazing bonnet to me! nice work! I could see a slight texture, but I'd say it's possible to simply flat that off and re-clear. maybe the reason the soric caused the texture was due to the outermost layer of carbon not being heavy enough? what gram was the outer layer?
great work again!
david
|