I have also seen print through with soric. If you can't post cure, you could leave the part under the sun for few days so the resins reach at maximum shrinkage and then sand flat and then reclear.
zacomposites
zacomposites
Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)
Group: Forum Members
Posts: 17, Visits: 1.8K
Warren (Staff) (09/05/2013)
If the texture was on the surface itself, not visible in the weave, then i would suggest the part needed longer in the mould.


didn't get u. u mean i should leave it a bit longer during curing time and then only debag?
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
If the texture was on the surface itself, not visible in the weave, then i would suggest the part needed longer in the mould.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
zacomposites
zacomposites
Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)
Group: Forum Members
Posts: 17, Visits: 1.8K
yeap. thats the one. the pic shown is after scnd time clear coat. i've wet sanded the first coat to remov the textured, but sure it wasn't good enough. maybe the third one will do. the first layer is 200g twill.
Edited 12 Years Ago by zacomposites
WilliamsHPF
WilliamsHPF
Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)
Group: Forum Members
Posts: 26, Visits: 349
Zacomposites,

  unfortunately I cannot see the defects you were talking about with the print through... the last few photos look like an amazing bonnet to me!  nice work!  I could see a slight texture, but I'd say it's possible to simply flat that off and re-clear.  maybe the reason the soric caused the texture was due to the outermost layer of carbon not being heavy enough? what gram was the outer layer?

great work again!

david
zacomposites
zacomposites
Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)
Group: Forum Members
Posts: 17, Visits: 1.8K
first attempt making mitsubishi triton bonnet.

method of process.

Top Part

method : infusion
reinforcement : 1 layer cf + soric 2mm + another layer 200 gm cf

lower part

method : wet layup
reinforcement : 1 layer of 300g csm + 1 layer 200g plain weave fiberglass( bolted area and hinge area being reinforced with more fabrics)

hinge is made by bending a metal rod.

bolted area i used pop nut rivet.

original weight : 15kg

After weight : 6.5kg

Problems occur

- soric pattern is imprint through. when first clear coat applied, can see diamond shape of soric.





Uploaded with ImageShack.us



Uploaded with ImageShack.us



Uploaded with ImageShack.us



Uploaded with ImageShack.us



Uploaded with ImageShack.us



Uploaded with ImageShack.us



Uploaded with ImageShack.us



Uploaded with ImageShack.us
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search