Message
carbonfibreworks
carbonfibreworks
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Below is an image of the mould for one side of the fairing, i have attached temporary flanges to it as i will not be able to cut the carbon to exactly the right size as the mould and this will allow me to trim it back to size. I have another fairing on production and will post more images later in the week.
Reply
Like
2
carbonfibreworks
carbonfibreworks
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Hi Warren
I have been able to get hold of an original mould for the bike fairing and although its polyester due to its age if should be ok, i have had to build temporary flanges around it and i am going to use an envelope bag. I will upload some images this eve of the mould.
Chris
Reply
Like
3
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Looking good. Make sure you put some pics of the fairing on here.
Warren
Carbon
Copies Ltd
Reply
Like
3
carbonfibreworks
carbonfibreworks
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
This is an upper section/tacho mount for a classic race bike, the original part in glass fibre weighs 350 grams and the carbon component is 80 grams. I used wet lay and vacuum bag. I will be making a complete fairing later this week for the same bike .
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Prev
1
2
3
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search