Chris (20/04/2013)
That's looking good, and very light too!!
Is there any gel coat or is it just resin?
I'm assuming that it's 2 halves that join at the front rather than the 1 piece?
Hi Chris
This was plain wet lay and vac bag and no gel coat and yes it will bbe made from 3 sections, the bike its being fitted to is a class winner and had four wins out of four races at the weekend and so reduced weight is our priority. It will have to be painted ( with a light coat) as classic bikes can not race with visible carbon.
Chris