mhdghoul
mhdghoul
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 49,
Visits: 113
yup i clear coat everything
best regards mhd alghoul 
mhdghoul@hotmail.com
youtube channel :atmospherejo link is
http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
Reply
Like
6
kylle
kylle
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 34,
Visits: 101
what kind of clear coat do you use?
Reply
Like
6
Warren
Warren
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 214,
Visits: 783
Here is a dinner plate I did a while ago:
Reply
Like
8
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Hi, Warren. Nice stuff.
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
6
Mr Rooty Tooty
Mr Rooty Tooty
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 15,
Visits: 156
Kylle, I use 2k automotive clearcoat sprayed through an HVLP gun.
Recently though I've been ordering it in a premix system. There's a company in the UK who do an aerosol can with an inbuilt catalyst. You pop a button on the base of the can, shake and then lay the paint down. Obviously once the can is activated you've got to use it all within about a couple of hours, and they aren't cheap.
http://www.specialistpaints.com/products/2k-clear-coat-canz
But tbh it's often better for me than getting all the compressor and paint equipment out and clearing the garage to spray HVLP.
Finish is good, I usually end up having to cut back with wet and dry and power buff up to a high sheen. It's not really possible to lay it down perfectly like you can with a gun (unless maybe if you're more talented than me
).
When carbon skinning I did use to get several layers of epoxy down, so that in the end I was sanding and buffing epoxy directly. But I found that even if you sand through to the carbon by accident, or only use a layer or two of epxoy over the cloth, or don't cut to like 1500 grit, if you lay down 2k clearcoat you get an excellent finish (as long as everything is flat).
Reply
Like
7
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Thx Mr Rooty Tooty for that 2K-in-a-can tip. Might be usefull for many of us
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
5
mhdghoul
mhdghoul
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 49,
Visits: 113
i use an automotive 2k hs clear coat , it is hard when fully cured and can easily be polished too , very glossy
best regards mhd alghoul 
mhdghoul@hotmail.com
youtube channel :atmospherejo link is
http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
Reply
Like
6
Bonobo
Bonobo
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
anybody here tried this one?
http://www.hbbody.co.uk/content/index.php?option=com_k2&view=item&id=101:496-autoclear-400ml&Itemid=27
i just got some but haven't tried it yet.
Reply
Like
6
Mr Rooty Tooty
Mr Rooty Tooty
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 15,
Visits: 156
First thing I skinned, ZX10r hugger (lessons learned!)...this is polished before clearcoat.
Then decided to do a full set of panels for a chap I know from a bike forum. A lot of issues to work out!
And the finished bike...
Now focusing back on carbon, skinning is way time consuming and messy!
Reply
Like
7
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Nice stuff
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
19
Prev
1
2
3
4
5
20
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search