Hi

What's the (nominal) thickness of the pre-formed tapes - the same as 2/2 195g cloth (.28mm)?

Looking at custom bicycle 'guards, so want an arc of circa 850mm length by 25mm width on a 280mm radius,  but the clearance between tyre and frame is ~1.5mm, so there's not a lot of room for multiple layers...
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The inside of the tape is release coated and must be applied to the resin.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
20130218ec
20130218ec
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 4, Visits: 10
Ta
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search