By 20130218ec - 2/18/2013 4:35:15 PM				
            
                      
            Hi
  What's the (nominal) thickness of the pre-formed tapes - the same as 2/2 195g cloth (.28mm)?
  Looking at custom bicycle 'guards, so want an arc of circa 850mm length by 25mm width on a 280mm radius,  but the clearance between tyre and frame is ~1.5mm, so there's not a lot of room for multiple layers...
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By 20130218ec - 2/25/2013 4:06:34 PM				
            
                      
            Ta
           
		 | 			
		 
	
	
						
		 	
		
	 |