Shouldn't be too bad, as it's linear arc.
QUICK QUESTION: The heat shrink tape - can't see any indication of whether it's interior or exterior face (with respect to a presented roll) that should be applied to epoxy layer, i.e. there's no adhesive on either side of tape - if this is so I take it either way up is OK, before applying heat...
|