Tape Thickness


Author
Message
20130218ec
20130218ec
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 4, Visits: 10
Hi

What's the (nominal) thickness of the pre-formed tapes - the same as 2/2 195g cloth (.28mm)?

Looking at custom bicycle 'guards, so want an arc of circa 850mm length by 25mm width on a 280mm radius,  but the clearance between tyre and frame is ~1.5mm, so there's not a lot of room for multiple layers...
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
LOL wear gloves then your fingers wont get so sticky!!!  When i do wetlay such as when making moulds, I end up changing them every 5-10 minutes as otherwise you end up in a goey mess and your fingers lift up the carbon youve just pressed into that tight hole.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Tags
20130218ec
20130218ec
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 4, Visits: 10
Shouldn't be too bad, as it's linear arc.

QUICK QUESTION: The heat shrink tape - can't see any indication of whether it's interior or exterior face (with respect to a presented roll) that should be applied to epoxy layer, i.e. there's no adhesive on either side of tape - if this is so I take it either way up is OK, before applying heat...
Edited 12 Years Ago by 20130218ec
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search