posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 107,
Visits: 504
http://www.menards.com/main/paint/caulking-sealants/silicone-caulk/white-lightning-flamebuster-intumescent-expanding-silicone-sealant/p-1496261.htm
this one i found on google
Edited
12 Years Ago by
neilb
Reply
Like
3
prsw
prsw
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 112,
Visits: 1K
matthieutje65 (05/02/2013)
thanks prsw, would be great!
update, nothing found yet, one company sent me to this:
http://www.dowcorning.com/applications/search/default.aspx?Ne=4294965469&N=4294949775&DCCD=PRODUCT&WT.svl=DC_home6&DCCT=PRODUCT
haven't had time to look trough it yet, feel free to do it..
The intended use could be for fire stopping seal in buildings, around pipes etc,
the silicone expands in heat and seals gaps and stops fire from spreading.
http://motoform.blogspot.se
Edited
12 Years Ago by
prsw
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
thanks prsw, would be great!
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
prsw
prsw
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 112,
Visits: 1K
Matthieu, I am looking in to this here in Sweden, hope to get back to you in a few days.
I also need it for some projects coming up.
BST carbon motorcycle wheels are made with this method.
http://motoform.blogspot.se
Reply
Like
2
neilb
neilb
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 107,
Visits: 504
i had a quick look on google and found a few but the temps at which it expanded at were quite high
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
I guess not...Silicone is normaly selfreleasing on most types of resins...
I it would be a problem I would add a selfreleasing film around the core, with some space to let it expand with the silicone
http://www.talkcomposites.com/1697/Thermal-compression-moulding
this is the post that sticked to my mind but havent found any answer on the silicone... I've send him an email yesterday but no answer yet...
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
Jack.Strong
Jack.Strong
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 52,
Visits: 549
Ive had a look as I am thinking of using the silicone mould for a plug.
Would the silicone stick to the curing composite ?
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
I will, but first I need to know which silicone to use and how much it will expand
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
Jack.Strong
Jack.Strong
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 52,
Visits: 549
Really interested in seeing how this goes Matthieu. Keep the thread updated.
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Hi,
I have a question,
I've been thinking about it for a long time and it has been on the forum yet, but not with the best results of information.
So I'm planning to make some tests with some silicone as an expanding core to get a nice outer finish with carbonfiber.
I plan to make a testsample of a tube made out of Carbonfiber:
- I plan to use an existing tube of metal
- Cut it in halve
- add some thickness (thickness of the carbonfiber, so not much) on the inside
- Put halves back together
- Fill the tube with silicone
- remove the silicone from the mould and remove thickness added before
- wrap wetted out carbon around the silicone
- Put it in an oven and hope for it to expand.
My question is, which silicone is expanding? mostly they make silicones that DONT expand because you dont want it to expand in most applications.
is it 1K silicone you'd better use or 2K silicone?
anyone has some experience with this?
I know about the blatter technique and so on, and thats not really what i'm looking for.
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Prev
1
2
3
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search