EF 80 Project


Author
Message
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Completed my first project using the EC EF80 Flexible Resin, mudguards for a Trials Bike. I am hoping that the combination of Carbon/Kevlar reinforcement and the Flexible Resin will hold up to the abuse of Trials Riding. I did do a very scientific "impact" test, put the rear one on the workshop floor and jumped on it ha ha.

Regards Warren

Carbon Copies Ltd
Edited 12 Years Ago by wozza
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
So 2 layers of 600g carbon?
I've read it's nearly impossible to Infuse with flexible epoxy resin?!
So would be vacuumbagging then? Did you use a gelcoat? I guess not?!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com