1/16/2013 8:11:18 PM
Completed my first project using the EC EF80 Flexible Resin, mudguards for a Trials Bike. I am hoping that the combination of Carbon/Kevlar reinforcement and the Flexible Resin will hold up to the abuse of Trials Riding. I did do a very scientific "impact" test, put the rear one on the workshop floor and jumped on it ha ha.
Regards Warren
By matthieutje65
-
1/17/2013 9:10:14 PM
curious about this infusion it, keep me updated
I'll first start with prepreg for my next project and after that I'll try using the flexible Epoxy