Group: Forum Members
Posts: 34,
Visits: 2.7K
|
Hi guys...I want to transition to prepreg and I'm trying to my head around some things before I invest...I'm not 100% sure prepreg will work in my very complex multi part mold so minimizing investment until I've got some confidence would be good. ...Big question is will I be able to get a decent indication of potential using XC110 in an oven that wanders either idea of setpoint by about 5 degrees? ...Another challenge is that the layup includes an already formed dry carbon panel on one of the mold parts, will the XC110 have enough resin to adhhere to that panel?
|