Hi guys...I want to transition to prepreg and I'm trying to my head around some things before I invest...I'm not 100% sure prepreg will work in my very complex multi part mold so minimizing investment until I've got some confidence would be good.
...Big question is will I be able to get a decent indication of potential using XC110 in an oven that wanders either idea of setpoint by about 5 degrees?
...Another challenge is that the layup includes an already formed dry carbon panel on one of the mold parts, will the XC110 have enough resin to adhhere to that panel?
Edited 3 Years Ago by chriscnf
Lester Populaire
L
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
chriscnf - 1/21/2023 8:51:22 PM
Hi guys...I want to transition to prepreg and I'm trying to my head around some things before I invest...I'm not 100% sure prepreg will work in my very complex multi part mold so minimizing investment until I've got some confidence would be good.
...Big question is will I be able to get a decent indication of potential using XC110 in an oven that wanders either idea of setpoint by about 5 degrees?
...Another challenge is that the layup includes an already formed dry carbon panel on one of the mold parts, will the XC110 have enough resin to adhhere to that panel?

I cannot comment on the temperature questions, I have no experience with the XC110 system.

In general i would have said that complex parts with multi part moulds is really the sweet spot for prepregs tho. If you want to bond to a core or to another cured panel, then I'd recommend using an additional resin film.

Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Lester is correct about the adhesive film.  Something like our XA120 would work well in most cases. 

In terms of oven temperature variation, its hard to say for sure. A few degrees here or there and you should be fine.  Significant variation for a significant period of time may well effect the resin flow characteristics thus impacting the cosmetic finish quality.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
chriscnf
c
Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)
Group: Forum Members
Posts: 34, Visits: 2.7K
Lester Populaire - 1/23/2023 9:54:23 AM
chriscnf - 1/21/2023 8:51:22 PM
Hi guys...I want to transition to prepreg and I'm trying to my head around some things before I invest...I'm not 100% sure prepreg will work in my very complex multi part mold so minimizing investment until I've got some confidence would be good.
...Big question is will I be able to get a decent indication of potential using XC110 in an oven that wanders either idea of setpoint by about 5 degrees?
...Another challenge is that the layup includes an already formed dry carbon panel on one of the mold parts, will the XC110 have enough resin to adhhere to that panel?

I cannot comment on the temperature questions, I have no experience with the XC110 system.

In general i would have said that complex parts with multi part moulds is really the sweet spot for prepregs tho. If you want to bond to a core or to another cured panel, then I'd recommend using an additional resin film.

Cheers Lester...it's the complexity of the joins that is interesting. The joining cloth has to double back almost 180 in a crucial area, I'm doing that fine with wet 200 twill and a silicone bladder with built in intensifiers. We shall see if I can make it work with prepreg...if not then I'll have to significantly change my product to make it work...I'll find a way I'm sure.

Edited 3 Years Ago by chriscnf
chriscnf
c
Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)Supreme Being (510 reputation)
Group: Forum Members
Posts: 34, Visits: 2.7K
Warren (Staff) - 1/23/2023 5:15:18 PM
Lester is correct about the adhesive film.  Something like our XA120 would work well in most cases. 

In terms of oven temperature variation, its hard to say for sure. A few degrees here or there and you should be fine.  Significant variation for a significant period of time may well effect the resin flow characteristics thus impacting the cosmetic finish quality.

Thats brilliant information...not bothered about cosmetics for now...if its functional than a good oven is justified.


Edited 3 Years Ago by chriscnf