Hi guys...I want to transition to prepreg and I'm trying to my head around some things before I invest...I'm not 100% sure prepreg will work in my very complex multi part mold so minimizing investment until I've got some confidence would be good.
...Big question is will I be able to get a decent indication of potential using XC110 in an oven that wanders either idea of setpoint by about 5 degrees?
...Another challenge is that the layup includes an already formed dry carbon panel on one of the mold parts, will the XC110 have enough resin to adhhere to that panel?
Edited 3 Years Ago by chriscnf
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search