Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Most infusion grade spray tacs are largely invisible. If they are causing you issues, you are probably using way too much. You don't need a lot - the vacuum should be doing most of the work. You just want to give a very very slight tac.
If you are really struggling, you can also try using an in-mould coating first, and then that will make your spray tac completely invisible regardless of how much you use.
|